Directional solidification and characterization of the Cd-Sn eutectic alloy
(ELSEVIER SCIENCE SA, 2007)
The Cd-67.8 wt.% Sn eutectic alloy was prepared by melting together appropriate amounts of cadmium and tin (both of 99.99% purity) in a graphite crucible in a vacuum melting furnace. Then, this eutectic alloy was poured ...